Shrinkage in propellant Manufactured by Solvent Process
Keywords:
Propellant composition, Solvent process, Single base propellants
Abstract
The propellant manufacturers select the dimensions of die-pin for extrusion of dough by trial and error method based on their experience. This paper presents a general equation applicable for any propellant composition processed by solvent process, in any shape, i.e., cord, monotubular or the multitubular. To illustrate the relationship, calculation for outer radius for a few typical single-base propellants is given.
Published
2013-01-02
How to Cite
Agrawal, K. (2013). Shrinkage in propellant Manufactured by Solvent Process. Defence Science Journal, 41(2), 131-136. https://doi.org/10.14429/dsj.41.4417